System 3 quick fair question
I will be using this to fill various dings on the bottom before I prime and paint. What is the recommended minimum temperature to apply this. I'm in the northeast and it still sucks up here, but I'd like t get this done so I can fish sometime in April. Thanks
|
I used a lot of it in temps down to around the mid fifties,to low sixties,and it cured fine,but naturally was a slower cure than the optimum temps in the 70's
Their spec sheet says 50 and above. Here's the link,or call Joe at Mertons. http://www.systemthree.com/reslibrar...ikFair_TDS.pdf |
Perfect. Thanks Big!
|