HA SCOTT
I FIRST USED 60 GRIT TO DO THE RUFF WORK THEN MOVED TO 150 GRIT ON THE PRIMER HAND AND BLOCK SANDING. I THINK IF I SAND THE FIRST TOP COAT WITH 220 OR 320 IT WILL LOOK JUST FINE BUT UNTIL I TRY IT JUST A GUESS FOR NOW. WITH STERLING YOU DON’T HAVE TO WORRY ABOUT REDUCING IT AFTER YOU START IT STAYS AT THE SAME CONSISTENCY FOR A LONG TIME. THEY SAY WITH AWLGRIP THAT IS A ISSUE. WHEN I DO THE HULL I WILL BE READY TO AT LEAST CLEAN THE BRUSH WITH THINNER AS I GO IF NEEDED.
FELLOW-SHIP [img]images/icons/grin.gif[/img]