View Single Post
  #5  
Old 03-26-2006, 04:54 PM
dcobbett dcobbett is offline
Senior Member
 
Join Date: Nov 2004
Location: Swampscott, MA
Posts: 299
Default Re: Tansom question for Hermco and others

HremCo,

I'm with clamsalot. I didn't realize you use a lot of new glass either.

Do you use just new glass (at least (4) 1708s and two 1-1/2 oz. mats) alone, or do you use it in combination with the old skin?

Starting at the new ply, working out, what's the thichness you are trying to get and what's the layup sequence, and does it change (total thickness and the sequence)if you are using just new glass vs incorporating the old glass skin into the layup?
Reply With Quote