Use the white colored 3M High Gloss Gelcoat Compound. It is of better quality and requires less work than the standard red colored 3M Superduty rubbing compound which is really designed for paint.

I think AquaBloc? makes a comparable product as well. Ask Offshore Systems on this site...I believed he has recommended it in the past.