Re: West System and Fuel
So far so good.
I sanded the area w/ a 120 grit grinder. Cleaned w/ acetone. Brushed on West System then added West System w/ micro balloons to consistency of mayonaise - put that on top w/ a nice thick bead. Let set overnight. Grinded smooth to a 1/4" thickness.
Fuel proof so far.
|