Got our resin in from US Composites and started laying some glass....started with the fast one.... we removed the bowpulpit and recored it, laid one layer so far of 1708, when that cures going to sand and add another layer, then fair it out. I then mixed some resin and wet out the transom plywood so that it might be in better condition and not soak up too much resin when I start our layup. I plan on doing 2 layers of 1708 on the outside (facing the bow) and one on the inside (going against the outerskin, which will already have a layer of 1708) I need pointers or advice here if I should use the aforementioned schedule or something else....better! Thanks