Finally got some work done on the boat. My dad came by and gave me a hand putting the top cap on and cutting out the new transom. Put the cap back on with 100 thru-bolts.
One set back lately has been some quickfair not setting off good. I know, I said it was some pretty good stuff. At first I had bought the 1.5qt kit and it was fine for the most part, sanded good, and not any soft spots. Then I went and bought the 1.5gal kit to finish the rest of the boat. I weighed it out on a set of scales, mixed it up with a drill paddle, heated my shed up with the heater and let it run for ever, and still had places that were completely soft. Now the outside of it before I started sanding was hard. Then after sanding a couple layers off, soft spots started appearing. I dont know if it was something I did wrong or just bad product. I do know that all the West Sytems 407 and 410 I have been using has not give me a bit of trouble. I ended up using some 410 to fill in the spots I had to grind out.
Just about finished with my wifes shop so I came focus on the boat some more.
Seacraft84
View Public Profile
Send a private message to Seacraft84
Find all posts by Seacraft84