Default 20. I have used the 26 but it is almost never needed anymore.

Quote:
Originally Posted by Blue_Heron View Post
That's not too bad. Is that for the Bluewater 20 or 26? Thinking of materials for my next project.
Dave
the decks the 20 is more then enough.One more thing to ad in using penske over okume plywood. To bond properly to wood you should use a thinner viscosity epoxy and always put a resin coat on first. With the penske it will bond with polyester or vinylester resin with out the wet out coat process and time.