Quote:
Originally Posted by Blue_Heron
That sounds like a good approach. As long as your bevel is at least a 12:1 ratio to your laminate thickness, and 6" should be plenty, your seam should be very strong. I would use epoxy resin for the tabbing for its superior secondary bond, but some guys here might consider that overkill.
Dave
|
We use epoxy for everything except where it is prohibited by class rules. Its not overkill in my book, just better boatbuilding!