Quote:
Originally Posted by Briguy
I'm bringing this thread back to life. What do I need to do to prep the awlgrip for the signature? I was thinking like 220 grit sandpaper.
Do I need to buff between coats? Will 3 coats be enough?
|
Brian
Try #320 It should be enough to scuff it. You DO NOT need to buff between coats. Scuff with a green 3M pad then wash & tag rag. Your now ready to to continue with the next coat. Two coats @ 8-2-4 mixture . If your not satisfied with the look, then add one coat 8-2-5 and then buff with 3m PERFECT-IT should do it