Some More Pictures. I added the foam and glassed with 1 layer of 1.5 oz csm for adhesion to foam. may be over kill but I never had problems with delam. added foam with some cabosil mixed with resin. then weighted down with buckets of water .let set- up ..Then one layer of 1808 0-90 and then another layer of drop scrap 1808 0-45 and 1708 0-45 .. abit frankinstien-ish as far as the glass goes. but I just have so much drop that it is getting in the way.
|