well I got a good start on the deck this weekend I got the duratec sprayed, 2 layers of mat down, and then the 3rd layer of mat and 1708 down. I needed help for the durtec and skin coat. So my my friend Mark came by and we kicked its ass. We sprayed the duratec and put the skin coat down in 2 hours. With 40 minutes of primer kicking off.
I cut all the glass the day before and had it rolled up and marked for laminating
Mark is the man with the cup gun. He has been doing this a long time, there was no sense in me getting in his way. I mixed and kept the cup gun fed. We used 1.5 gallons of duratec for the deck build
here is how we set the mat to laminate, when the flop over they are over lapping by about an 1"
__________________
36' Yellowfin
1972 20' seacraft 140 suzuki
http://www.classicseacraft.com/commu...ad.php?t=18607
billythekid
View Public Profile
Send a private message to billythekid
Find all posts by billythekid