oh, makes sense.

Do you think the film material is necessary or do you use it just for insurance? I have just relied on 5-6 coats of mold release wax and I have had good luck with just that so far. I would like to try PVA and see if it helps the release on more complex parts but didn't think I would be necessary on a flat part like the deck.