Quote:
Originally Posted by gofastsandman
Well, I am a walking cartoon and can voice many of our favorites.
General has given their blessing on the welds and work done.
They will make it what I want and are a pleasure to work with.
Mine was tested at 5 lbs. General said 2-3 is fine.
They didn't like plug welds on top of the baffles but said they would not
cause corrosion issues.
CG said there is no ABYC on rec boats, but they would flag his pickups on
any for hire vessel. Only alum or ss is Comm ABYC.
|
tank coating:
clean,scuff sand,clean again,followed by a chemical etch prime,then coat it in interprotect 2000 - correct thickness.set the tank on strips of starboard."rough up" the starboard and glue it down to the hull - AFTER you test set the tank,to determine if the tank sits level....
this is the way to go !