Christmas came early again in the form of material order from forum member shine's store Gulfstream Composites.



General rundown of materials is:
  • 30 gallon kit (which is shipped as (5) 6 gallon kits) of Raka Epoxy with the 350 non-blush hardener
  • 50 yards of 50" wide 1708 (125lbs of cloth)
  • 10 yards of 50" wide 12 oz Biaxial cloth (will use to make tape for tabbing, etc)
  • 10 yards of 50" wide 6oz cloth (for laying down tight radii on hatch lids, hatch gutters, etc)
  • 2.5lbs of Cabosil
  • 5lbs of Wood Flour
  • 3" and 6" lamination rollers
  • Lots of mixing cups, chip brushes, and foam rollers

I guarantee I'll have to put in another other of materials at some point but I should be good on most stuff for a long while. Start cutting tonight!
You will use it all and then some