I used Coosa 20, because I did not realize there was a 26 when I bought it. I had to rent a truck and drive to Maine to pick it up. Not sure if I would use the 26 if I had to do it over again. When you hit the 20 with a hammer it surely does not dent very easily.

I have started doing core replacement on the under deck storage boxes and the bottom of the cap. I am using 1/2 Scored Divinycell. I decided to leave the original balsa coring, at the bow, as I am a little worried about losing the shape of the crown in the deck. It looks like it will be after thanksgiving before I get the cap and bow liner back in the hull.

Still making it up as I go along.