View Single Post
  #68  
Old 07-01-2022, 09:15 PM
Xcomunic8d Xcomunic8d is offline
Recovered
 
Join Date: Oct 2016
Posts: 320
Default

Yeah what dirt said. I catalyze real low here too. I try to wait for days where it should get hot in afternoon to help. I use mainly poly though. .75-1.25% depending on temps.

As to vertical surfaces. I paint some in with chip brush, wet out my stuff and get to it with a spreader, then roller. Walmart started selling bondo jelly resin. I’ve never used it but that would be a ton easier… and yes voids are lousy. I had some. Drilled holes and injected filler with a caulk gun. They sell tubes at west marine you can load and squeeze in there
Reply With Quote