Re: Seacraft Surgery 2
Ha Jimmy
I think it was called Blue Mist I would have to look at my chart or old can’s of paint to confirm. As for the fairing compound I used the West Systems fairing compounds I used several types depending on if I was doing heavy glass work or top finish fairing work. I used the Sterling two part primer first before I painted both inside and out of the boat it sands very well before you paint over it. I would use a foam roller with the primer process, when you use a paint brush you usually will make streaks that will have to be sanded more aggressively to get even.
FellowShip [img]images/icons/cool.gif[/img]
|