John,
I would go with the two pound density.I believe this is what was used in the original builds,and is the most common pour foam stocked by most fiberglass dealers.
The structural strength came from the fiberglass boxes laminated into the hull.The foam is there for flotation and to displace air so that any water can't fill that space,and sink the boat.(just my opinion).
__________________
All this,just for a boat ride
Reply With Quote
 

Thread Tools Search this Thread
Search this Thread:

Advanced Search
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 03:33 PM.


Powered by vBulletin® Version 3.8.7
Copyright ©2000 - 2025, vBulletin Solutions, Inc.
All original content © 2003-2013 ClassicSeacraft