Is this a one time shot or production where you are doing many of the same part?
Are you going to be Resin Infusing the glass or bagging down pre wet glass?
You can use visqueen, Tacky tape, the flow media and breather can be found at a fabric shop. if you are infusing then you will have to use reinforcements that allow flow and low viscosity resins. If you are hand catalyzing and not using metermix pumps use a slow resin and or refridgerate before catalyzing to give you plenty of time to pull the resin through the whole part.
__________________
I heard it on the coconut telegraph..........
Reply With Quote
 

Thread Tools Search this Thread
Search this Thread:

Advanced Search
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 08:18 AM.


Powered by vBulletin® Version 3.8.7
Copyright ©2000 - 2025, vBulletin Solutions, Inc.
All original content © 2003-2013 ClassicSeacraft