Nice work!

I just got done with my Duratec vinylester primer experiment. It kicks quickly and sticks to anything. I stuck it to high microbaloon content epoxy (a no-no) and gel coated over top of it and it all seems good so far. And the vinylester primer is high build. .040" per application! I put it on with a roller and it left a texture in the most wicked way, as I couldn't let it just lie flat, plus I ran out of short nap rollers. It just about matches the stock(?) off white/light sand color in my 1974 Master Angler. I wish I had sprayed it, as I would have just left it. It matches the existing oxidized gelcoat pretty well.

Last edited by FishStretcher; 05-13-2012 at 09:31 PM.
Reply With Quote
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 01:48 AM.


Powered by vBulletin® Version 3.8.7
Copyright ©2000 - 2025, vBulletin Solutions, Inc.
All original content © 2003-2013 ClassicSeacraft