Default lamination schedule question

I'm doing some laminating with 2 layers of 3/4 coosa/penske and west system epoxy.
Couple of questions for you glass gurus:

Do I need to put a layer of glass between the layers of coosa/penske (mat, 1708, straight cloth), or just thickened epoxy?

After putting down a layer of 1708 (mat side down) do I need to put a layer of mat (epoxy compatible if I can find it) on the cloth side of my 1708 before putting down the next layer of laminate (if the next layer is not 1708, but is coosa/penske or outside skin)?

Is 1708 sufficient for tie-ing together old skin and existing hull (after a nice 12:1 scarf)?
Should I finish with a layer of straight cloth to make fairing a bit simpler? What weight?

I've been searching the forums for hours, and these are the only questions I have left.
Thanks!
__________________
Zachary

[SIGPIC][/SIGPIC]

Last edited by erebus; 02-03-2013 at 07:55 PM. Reason: edited for accuracy.
Reply With Quote
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 02:24 AM.


Powered by vBulletin® Version 3.8.7
Copyright ©2000 - 2025, vBulletin Solutions, Inc.
All original content © 2003-2013 ClassicSeacraft