You are fine. That is nothing to worry about. No squeege, use a laminating roller and a 3/8 nap paint roller to wet it out then lay your 1708. Smooth out with the paint roller then go to the laminating after about 7-10 minutes. You need the resin to dissolve the starches in the fabric so it has no memory left it before you start with the laminating roller. Also if you are laying smaller stuff up put a piece of mat behind the 1708, it will solve the problem of the little air bubbles.
__________________
36' Yellowfin
1972 20' seacraft 140 suzuki

http://www.classicseacraft.com/commu...ad.php?t=18607
Reply With Quote
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 08:51 PM.


Powered by vBulletin® Version 3.8.7
Copyright ©2000 - 2025, vBulletin Solutions, Inc.
All original content © 2003-2013 ClassicSeacraft