Default Laminateing resin.. aka no wax polyester

Hey I have a small delima.. I mixed some fairing with my laminating resin instead of the standard boat yard stuff.. as you know it's tacky as all get out... I have left it in the sun as much as I could and also waited a good month before I sand... Well it's still tCky....What can I do to it to seal it so it isn't tacky anymore? Can I just roll some regular boat yard resin over i? Will it convert I to hardened upso I can sand it ...I don't have enough sand paper on this Earth to sand the tacky stuff.. oh and yes I did use the correct hardner amounts..thanks guys
Reply With Quote
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 05:22 AM.


Powered by vBulletin® Version 3.8.7
Copyright ©2000 - 2025, vBulletin Solutions, Inc.
All original content © 2003-2013 ClassicSeacraft