Default Re: 1971 20 SF Transom project

Have today and tomorrow off from work, so I went to the lumber yard and picked up 2 sheets of marine ply. They charged me 92.00 per sheet. Other yards around had similar prices so i figured it wasn't too steep. Also, got all my fiberglass supplys from LBI in groton CT. I have to say, there website is very easy to understand if your a novice in buying fiberglass.

I just have a couple last minute questions before I start to lay it up....I plan on building up the outer skin with a couple layers of glass, and I would to know whether or not I have to wait for each layer to cure completely, or can I just wait an hour or so to lay the next on?
Here is my plan for the transom...

outerskin
1.5 oz mat
1708
1708
wood
1.5 oz mat
wood
1.5 oz mat
24 oz woven
1708
6oz cloth

Am I going overboard with all the layers of glass, or should I have more?....all opinions welcome. Thanks
Reply With Quote
 

Thread Tools Search this Thread
Search this Thread:

Advanced Search
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 12:18 PM.


Powered by vBulletin® Version 3.8.7
Copyright ©2000 - 2025, vBulletin Solutions, Inc.
All original content © 2003-2013 ClassicSeacraft