The reason I used Get Rot was the fact it is so light and will run - I do wish I knew more about using fiberglass resins and cloth - just said that tonight btw for pulling an old thru hull transducer and filling the hole.

Just a little FYI for some other guys as dumb as me and have some small soft spots.
__________________
Any way you measure it - dumbass is expensive
Reply With Quote
Reply


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 07:52 AM.


Powered by vBulletin® Version 3.8.7
Copyright ©2000 - 2025, vBulletin Solutions, Inc.
All original content © 2003-2013 ClassicSeacraft