I guess the 5200 will do the job,it's strong stuff no doubt.When I did mine,I laid up two layers of 1708 to the inner transom skin,as it was pretty thin.That kind of surprised me,that Seacraft didn't make it a bit thicker.
I then used a a notched trowel to spread a thickened batch of System Three epoxy resin to the new marine ply transom.
We clamped and fastened it into place and let it cure.
I did all the rest of the glass layup on the new transom and stringer tie ins with 1708 and polyester resin.The two resin systems never came into contact with each other so there was no curing problems.
I just had so much rotted core on everything else that i went with polyester.It, for me at least is much easier to wet out the fabric,and work with,and also less money than epoxy.
__________________
All this,just for a boat ride
Reply With Quote
  #2  
Old 03-05-2012, 07:03 PM
Entourage Entourage is offline
Senior Member
 
Join Date: Dec 2007
Location: Fairhaven Mass
Posts: 583
Default

Here is mine 4 layers on inside 1 mat 3 1708
Attached Images
  
Reply With Quote
Reply


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 09:31 AM.


Powered by vBulletin® Version 3.8.7
Copyright ©2000 - 2025, vBulletin Solutions, Inc.
All original content © 2003-2013 ClassicSeacraft