Delamination of about 6" of the hull to side tabbing. Delamination of the top hull side stiffener. Delamination of about top 5" of fiberglass box frame.

No surprise the hull vent patch came out, it was not even glassed on the inside and just some matt on the front. The was work already done when I bought the hull. Would have been OK if not for this impact.

there is also some cracking of the fairing compound between the tow hull side stiffeners, but it does not appear to be very bad. My plan is to fix the delamination now, return the stiffness, then use the boat until winter when I can cosmetically make it look new again. Unfortunately, I am going to eventually need to re-paint the whole port side on the out side and a few section on the inside. :x


damage pictures....





yesterday I ground out the delmainated glass, and then back up the stiffener and the frame so the new glass will have plenty of overlap to bite

[/quote]
Reply With Quote
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 04:22 PM.


Powered by vBulletin® Version 3.8.7
Copyright ©2000 - 2025, vBulletin Solutions, Inc.
All original content © 2003-2013 ClassicSeacraft